Anttila EJ et al. - Unfilled polymer resin had the highest polymerization shrinkage of 0.84%. Unidirectional FRC had a relatively high shrinkage in the transverse direction with respect to the reinforcing fibers (0.41%) whereas the shrinkage along the reinforcing fibers was small (0.02%). Bidirectional FRC showed a low shrinkage value (0.03%). For most tested materials the hydroscopic expansion seemed to compensate for the polymerization shrinkage.
Today in Dental Materials...keeping you current
Receive free subspecialty "5-minute updates" via email
Randomized Controlled Clinical Trial of Zirconia-Ceramic and Metal-Ceramic Posterior Fixed Dental Prostheses: A 3-year Follow-up
The International Journal of Prosthodontics, 11/19/09
Factors Affecting Survival and Usefulness of Implants Placed in Vascularized Free Composite Grafts Used in Post–Head and Neck Cancer Reconstruction
Clinical Implant Dentistry and Related Research, 10/28/09
Dental Enamel Irradiated with Infrared Diode Laser and Photo-Absorbing Cream
Photomedicine and Laser Surgery, 11/05/09

See Latest Articles