Shear Bond Strength of Brackets Bonded to Enamel with a Self-Etching Primer
Angle Orthodontist , 08/15/08
Pithon MM et al. - There were no significant differences between the SBS of groups 0, 1, 3, 7, and 15 However, those groups had higher SBS compared with groups 21 and 30. No significant difference was observed between groups 21 and 30. Despite the decrease in SBS for groups 21 and 30, bond strength values were still satisfactory.
| Previous Article | Next Article |
Today in Dental Materials...keeping you current
Receive free subspecialty "5-minute updates" via email
Investigation of contact allergy to dental metals in 206 patients
Contact Dermatitis, 06/09/09
Physical and Compositional Changes on Demineralized Primary Enamel Induced by CO2 Laser
Photomedicine and Laser Surgery, 06/30/09
Solubility of TTCP and beta-TCP by solid titration
Archives of Oral Biology, 06/09/09
Article Search
Sponsor


See Latest Articles