Microshear Bond Strength of Resin Bonding Systems to Machinable Ceramic with Different Surface Treatments
The Journal of Adhesive Dentistry, 06/19/08
Xiangfeng M et al. - For three RBSs, bond strength at TC 0 was not affected, regardless of ceramic surface treatment. All combined groups of ceramic surface treatment and resin bonding system decreased after 10,000 thermal cycles, especially groups treated with alumina blasting and bonded with each of three RBSs. MBS/HB/VLIIHV with each surface treatment did not improve the bond strength and durability compared with MBS/VLIIHV.
Today in Clinical Pharmacology...keeping you current
Receive free subspecialty "5-minute updates" via email
Combined topical dexamethasone/tacrolimus therapy for management of oral chronic GVHD
Bone Marrow Transplantation, 11/05/09
Ketoprofen 2% Oral Gel
U.S. Pharmacist, 11/06/09
Effectiveness of 0.50% and 0.75% chlorhexidine dentifrices in orthodontic patients: A double-blind and randomized controlled trial
American Journal of Orthodontics and Dentofacial Orthopedics, 11/10/09
Today in Dental Materials...keeping you current
Receive free subspecialty "5-minute updates" via email
Dental Enamel Irradiated with Infrared Diode Laser and Photo-Absorbing Cream
Photomedicine and Laser Surgery, 11/05/09
Clinical and Histological Evaluation of Granular Beta Tricalcium Phosphate for the Treatment of Human Intrabony Periodontal Defects. A Report on Five Cases
Journal of Periodontology, 11/06/09
Factors affecting the shear bond strength of metal and ceramic brackets bonded to different ceramic surfaces
European Journal of Orthodontics , 11/11/09

See Latest Articles