Determining the complex modulus of alginate irreversible hydrocolloid dental material
Dental Materials, 05/09/08
King S et al. - The results indicate that the MFR is capable of recording the complex shear modulus of alginate irreversible hydrocolloid for 60 min from the start of mixing and to simultaneously report the changing visco-elastic parameters at all frequencies between 1 Hz and 100 Hz. The storage modulus shows a dramatic increase to 370% of its starting value after 6 min and then reduces to 55% after 60 min. The loss modulus increases to a maximum of 175% of its starting value after 10 min and then reduces to 94% after 60 min.
| Previous Article | Next Article |
Today in Dental Materials...keeping you current
Receive free subspecialty "5-minute updates" via email
Investigation of contact allergy to dental metals in 206 patients
Contact Dermatitis, 06/09/09
Physical and Compositional Changes on Demineralized Primary Enamel Induced by CO2 Laser
Photomedicine and Laser Surgery, 06/30/09
Solubility of TTCP and beta-TCP by solid titration
Archives of Oral Biology, 06/09/09